ABISCLALD kayan da aka sake na acrylonitrile, butryDene, butdadiene, da Styrene, wanda shine samfurin copolymerization na waɗannan monayoyi uku. An kira shi bayan harafin farko na sunayensu na Ingilishi. Yana da ci gaba mai ƙarfi, mai kyau, da kuma kyakkyawan aiki, amfani da shi azaman filastik filastik. Abs filastik
A masana'antu, polybutadieneen latex ko Styrene butteradiene tare da ƙarancin m styrene ana amfani da shi azaman babban sarkar da monresremer. A zahiri, yawanci cakuda polin graft dauke da fayedadene da acrylonitrile Styrene coollymers San ko kamar yadda. A cikin 'yan shekarun nan, daban-daban Abs resins ya dace da aikace-aikace daban-daban an kuma shirya su da monomers pyres da acrylonitrile monomermerized a cikin tsari daban-daban. An fara samar da masana'antu a tsakiyar shekarun 1950 a Amurka.
1. Abubuwan Amorphous, tare da matsakaici na matsakaici da babban danshi na danshi, dole ne a bushe sosai. Filayen filastik wanda ke buƙatar babban surshe dole ne a sami preheated da bushe na dogon lokaci a 80-90 digiri Celsius na 3 sa'o'i
2. Yana da kyau a yi amfani da zafin jiki mai yawa da zazzabi mai yawa, amma idan kayan zafin jiki ya yi yawa, yana da sauƙin lalacewa (lalata digiri na 270). Don sassan filastik mai zurfi, zazzabi ya kamata a saita shi a digiri 50-60, kuma don sassan filastik mai tsayayya da ƙasa, ya kamata a saita zazzabi mai tsayayyen wuta, ya kamata a saita zazzabi mai tsayayye .as
3. Don magance matsalar matakan ruwa, ya zama dole don inganta motsi na kayan ta hanyar yawan zafin jiki, zazzabi mai yawa, ko canza matakan inlet na ruwa .c ko abs
4. Idan kayan zafi ko kayan wuta masu zafi suna kafa, samfuran lalata filastik zasu ci gaba da kasancewa a farfajiya na ƙwararrun ƙirar bayan kwanaki 3-7 na samarwa don haskakawa. Mormold yana buƙatar tsabtace a cikin wani lokaci, da manyan munanan buƙatar da za a ƙara su zuwa mold surface.pc ko abs